Spellbound, 9 inch tall fine art equine sculpture custom glazed by Hyn Patty to a dark dappled bay - shown here taking first place in each of his classes and then went on to be awarded Reserve Champion of his division at Shay Canfield's all china equine sculpture show, May 27th, 2023 in Virgina.  Earthenware bisque with underglaze fired at cone 04, satin clear glaze fired at cone 06, overglazes (china paints) fired at cone 016.   Private collection of the glazing artist.