DSC_5543-2.jpg
In this small balls I use commercial glazes. This was my first firing.
Faring renge 1220-1280C / Oxidizing Atmosphere
Photo Information
- Taken with NIKON CORPORATION NIKON D600
- Focal Length 100 mm
- Exposure Time 1/125
- f Aperture f/8.0
- ISO Speed 800