Marcia Selsor 1,981 Posted January 7, 2020 Report Share My Faux celadons recipe Posted this recipe years ago Selsor Faux Celedon ^6 Oxidation Whiting 18.5 Neph Syen 25.8 EPK 18.8 Silica 31.1 Gerstley B 4.6 total. 98.8 Copper carb 0.3 Mason #6600 Black 0.02 Hulk 1 Quote Link to comment