dhPotter 472 Posted April 10, 2019 Report Share Love the pastel colors. Looks like some crystal growth also. 1515art 1 Quote Link to comment
1515art 260 Posted April 11, 2019 Report Share 15 hours ago, dhPotter said: Love the pastel colors. Looks like some crystal growth also. Tx, I’m having a hard time warming up to them actually these are not glazes that I picked ou and while I think they are OK my eye wants to focus on any defect. Eventually I’ll adjust, the cream colored vessel has a nice silky texture, although I’d prefer slightly more distinct iron specks. Quote Link to comment