Could you go for a visual image on the book, like the look of a tooled leather cover rather than words? I don't think it is as likely for a buyer to be drawn to the dish by the words as that a buyer would decide against the purchase because of the words. But then, I have never bought a greeting card in which words are already printed in it. 

Link to comment

Sadly the cassius body decided to warp even more, it was already a bit warped as it dried. I'll keep it as a test and not waste the clear glaze on it. However the slip painting did turn out perfectly, looks about the same as on the greenware photo here. 

Edited by yappystudent
Link to comment

Sorry to hear that.  He is a great image...looking forward to see the next one.   On the warping, I usually take a very long time to dry my stuff.  I leave it wrapped in plastic letting only a little air in then slowly bring it out.  Not unusual for me to dry something for more than a month sometime 2 months.  (I do like making tiles and low bowls). 

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.