PotsbyChar Posted February 21, 2011 Report Share Posted February 21, 2011 Is there a way that a studio potter can glaze the entire piece at cone 10? Any stilts out there that will withstand those high temps? I see commercial wares that are glazed all over. So I am just wondering if that option is available to studio potters. Any advice will be greatly appreciated. Thanks Charlotte Link to comment Share on other sites More sharing options...
Marcia Selsor Posted February 21, 2011 Report Share Posted February 21, 2011 what you need to do is have stilts that shrinks with your piece OR bisque at the same temperature as your glaze. Some manufacturers do this. Marcia Link to comment Share on other sites More sharing options...