cp dunbar Posted February 8, 2011 Report Share Posted February 8, 2011 Looking for a recipe. the color is about the same as copper that has oxidized. The result is a variegated color that varies from a turquoise to almost black spots. Link to comment Share on other sites More sharing options...
pixie1035 Posted February 16, 2011 Report Share Posted February 16, 2011 Looking for a recipe. the color is about the same as copper that has oxidized. The result is a variegated color that varies from a turquoise to almost black spots. i use this cone 6 glaze all the time... tried and true TurquoiseNeph SyStrontiumFlintBall ClayLithiumTotal Also add:Copper CarbBentoniteEpson SaltComments:Very bright. Very turquoise, Matt, breaks black. Moves a lot if applied too thick. Create rough antique look a like texture. Link to comment Share on other sites More sharing options...