Mark C. Posted October 19, 2014 Report Share Posted October 19, 2014 I was doing my every 4-5 year wash job and I was loading up some bowls with epk for calcining for my wash formula. Heres how I do it in some green bowls as well as one cracked bisqued one I use just for this purpose . You can use whatever form you have as it all just comes out and after you blow or towel out the form its ready to glaze. Mark Link to comment Share on other sites More sharing options...
phill Posted October 25, 2014 Report Share Posted October 25, 2014 great thanks for posting this! love the picture too! Link to comment Share on other sites More sharing options...