sad duck    0

Can any one help? I've bubbles on the rim of my chip & dip dish. I have fired it twice and the things just keep moving around the rim. Looks like they are little spots where you can see the unglazed clay in the middle of it. This is a wedding gift next month, Please help is you know how to fix this, sad duck

Share this post


Link to post
Share on other sites
Icyone2    0

I've had some luck dremmling the sharp burst bubbles and lightly glazing the bare bisque if any and firing at a cone lower.

 

when I fired at same temp I just got more bubbles elsewhere.

 

I'm no expert though just had to get used to new type of glaze recently and it did not like it being very thick at all.

Share this post


Link to post
Share on other sites
sad duck    0

I've had some luck dremmling the sharp burst bubbles and lightly glazing the bare bisque if any and firing at a cone lower.

 

when I fired at same temp I just got more bubbles elsewhere.

 

I'm no expert though just had to get used to new type of glaze recently and it did not like it being very thick at all.

 

 

 

yes i ws just thinking of lower the Kiln to slow instead of Medium maybe that would do it, Thanks for the in put!!!!!

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×