centered Posted December 12, 2010 Report Share Posted December 12, 2010 with my new zen raku kiln i purchased a pyrometer. where does the pyrometer probe go? where does it get attached? do i put it between some bricks or in the side hole on the kiln? thanks Link to comment Share on other sites More sharing options...
Marcia Selsor Posted December 12, 2010 Report Share Posted December 12, 2010 Put it in the side hole of the kiln, if that is a peep hole. You want it near where the glazes are. Marcia Link to comment Share on other sites More sharing options...