Posted 01 April 2013 - 12:13 PM

If I use a matt glaze from company "A" and then add a clear gloss from company "B" will it cause the finish to become toxic or will it stay food safe?

#2 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,671 posts
  • LocationNorthern Virginia

Posted 01 April 2013 - 12:55 PM

Any time you overlap two different glazes . . . you create a new, third glaze. And, depending on the contents of the two glazes, you could end up with an unstable/nondurgable glaze that leeches a coloring oxide, etc. Doesn't matter if the glazes were made by two different companies or the same company. Putting a "safe" clear over a "problem" glaze will not automatically make the resulting glaze safe . . . you need to test it.

#3 Fish Lady

Fish Lady

    Newbie

  • Members
  • Pip
  • 4 posts

Posted 01 April 2013 - 01:14 PM

Any time you overlap two different glazes . . . you create a new, third glaze. And, depending on the contents of the two glazes, you could end up with an unstable/nondurgable glaze that leeches a coloring oxide, etc. Doesn't matter if the glazes were made by two different companies or the same company. Putting a "safe" clear over a "problem" glaze will not automatically make the resulting glaze safe . . . you need to test it.



How do I test to see if it has become toxic?

#4 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,671 posts
  • LocationNorthern Virginia

Posted 01 April 2013 - 01:46 PM


Any time you overlap two different glazes . . . you create a new, third glaze. And, depending on the contents of the two glazes, you could end up with an unstable/nondurgable glaze that leeches a coloring oxide, etc. Doesn't matter if the glazes were made by two different companies or the same company. Putting a "safe" clear over a "problem" glaze will not automatically make the resulting glaze safe . . . you need to test it.



How do I test to see if it has become toxic?



Here's a start: http://digitalfire.c...achable_12.html

Also, consider picking up a copy of John Hesselberth/Ron Roy's "Mastering Cone 6 Glazes". The bible for making durable, stable glazes and how to test them at home.

#5 Fish Lady

Fish Lady

    Newbie

  • Members
  • Pip
  • 4 posts

Posted 01 April 2013 - 04:18 PM



Any time you overlap two different glazes . . . you create a new, third glaze. And, depending on the contents of the two glazes, you could end up with an unstable/nondurgable glaze that leeches a coloring oxide, etc. Doesn't matter if the glazes were made by two different companies or the same company. Putting a "safe" clear over a "problem" glaze will not automatically make the resulting glaze safe . . . you need to test it.



How do I test to see if it has become toxic?



Here's a start: http://digitalfire.c...achable_12.html

Also, consider picking up a copy of John Hesselberth/Ron Roy's "Mastering Cone 6 Glazes". The bible for making durable, stable glazes and how to test them at home.



Thank you... I currently have one dish with a lemon and another with vinegar.

#6 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,125 posts
  • LocationWilton, NH USA

Posted 01 April 2013 - 04:36 PM

Thank you... I currently have one dish with a lemon and another with vinegar.


Note that those are only "rule in" tests not "rule out".

If they fail that test, you have no need to run a lab test. If they PASS that test, it does NOT say that it will not leach components. Only a standard acetic acid leach test will do that. (lab testing)

Note that if the glaze does not contain any toxics, then there is no need to test. It might be "bad" glass...... and deteriorate in visual character over time and use..... but it will not harm anyone.

best,

.......................john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#7 Iforgot

Iforgot

    Advanced Member

  • Members
  • PipPipPip
  • 155 posts
  • LocationColorado

Posted 05 April 2013 - 10:35 PM

What color is the matte glaze from "A" company?



Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit

#8 Fish Lady

Fish Lady

    Newbie

  • Members
  • Pip
  • 4 posts

Posted 06 April 2013 - 05:03 PM

Alabaster