I recently got a used kiln and got it up and running this week. I did a test fire and it was able to reach cone 05 within an hour and fifty minutes. Yesterday, I decided to do a bisque fire. I started it at 7:30 and it seemed like the firing was going pretty good until the last part. I noticed that when I glanced in the peep hole that the top elements were not glowing at all. I know I need to replace them. I had the kiln going for at least 12 hours and it still hadn't reached cone 04 so then i decided to just turn it of and let it be. Today, when I looked at the cone there wasn't even a slight bend in it. What do I do about my bisque ware? When I change the elements should I re-fire them? Or since it was in the kiln for so long and the top elements gave up at the last bit that the bisque ware is okay and I don't have to re-fire? If someone could help me out an answer my question that would be great. Thank you.

 

-Lisa

Share this post


Link to post
Share on other sites

Honestly, there is no harm in re-firing it. I've refired bisque-ware many times (if you get wax on it, etc). I'd rather do that than have excessive carbons / organic materials that didn't burn out during bisque outgass during the glaze firing.

Share this post


Link to post
Share on other sites

While you are ordering your new elements, order some self supporting witness cones too.

If you fire Cone 04 bisque, get 03, 04 and 05, ... if you glaze fire to 6, get 5, 6 and 7. I put a set of these at the bottom, middle and top shelf of my kiln for each firing.

This bracketing of your final Cone temp will give you a way of knowing what happens on every level of your kiln so you would not have to guess and worry about re-firing.

Share this post


Link to post
Share on other sites

You don't need to refire; although the bisque will be more porous than if you had reached ^05. Before glazing I'd wipe them down with a wet sponge so the bisque does not absorb too much glaze -- wipe one item and then glaze, not wipe all the wares and then glaze. Depending upon the clay body, some potters bisque as low as ^010 and as high as ^02. Bisqueing is just to burn out organic impurities and provides some hardness to the wares for handling during glazing.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.