glaze mataerial substitutions ?

Recommended Posts

I mixed up a test batch of Steven Hill's Strontium Crustal Magic -

Cust Feld 40.0

Whiting 15.2

Stontium Carb 11.1

EPK 13.1

Frit 3124 4.0

Lithium Carb 4.0

titanium Diox 12.1

 

Yellow iron ox 2.5

Bentonite 2.0

 

But I don't have all of these so this is the recipe that I mixed

G200 40.4

Whiting 15.2

Strontium Carb 11.1

EPK 13.1

Frit 3124 4.0

Lith Carb 4.0

Titan Diox 12.1

 

Red iron ox 2.5

Ball Clay 2.0

 

What do you think the differences will be?

Share this post


Link to post
Share on other sites

It is always good to test. I have used Black iron with some interesting results for yellows. Yellow iron is sometimes substituted for yellow umber. You may have to make some alterations and see what happens. Will you have time to test?

 

Marcia

Share this post


Link to post
Share on other sites

The bentonite is in there to prevent the glaze from settling in the bucket, and also to help the glaze fit the pot for raw glazing. You could even leave it out. The Red Iron Oxiide is more crucial. It will give you a darker colour than the yellow. You could try dropping it down to 1% in a line blend as a test before you mix your batch.

Tom Roberts.[TJR]

Share this post


Link to post
Share on other sites

Yes I will test

unfortunately I have added water and can't decrees the percentages.

I believe Steven Hill does single fire many of his pieces, so that may be what the bentonite is for.

Share this post


Link to post
Share on other sites

I have single fired this glaze and used a Australian available potash feldspar that comes from India and it worked fine. I think it needs some oxides to give i ta bit more life. I put less around the bottom third of the pot and it didn't run and added an oribe around the top, over the crystle magic, whcih ran down a small amount. I looks quite nice.

 

Lynette

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.