CPT Posted November 6, 2012 Report Share Posted November 6, 2012 Help! Has this happened to anyone? When I did a Cone 06 fire, I had pieces of firebrick fly off and stick to my glazed pottery! I then get these little 'burrs' in my beautiful work and I have to sand them off. I just vacuumed the heck out the inside of my kiln again, so hoping that will solve this ongoing issue. Any other advice? Thanks. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted November 6, 2012 Report Share Posted November 6, 2012 Are the pieces coming from a lid that is not in good shape? Marcia Link to comment Share on other sites More sharing options...
TJR Posted November 7, 2012 Report Share Posted November 7, 2012 I am agreeing with Marcia. There isn't any reason for soft brick bits to fly sideways, so check your lid for pieces falling off.You could put a shelf above your glazed ware, but chances are pretty good that you need to replace the lid. TJR. Link to comment Share on other sites More sharing options...
Kabe Posted November 7, 2012 Report Share Posted November 7, 2012 This is a long shot and probably not right. Is there anyway a vent for the kiln (If you have a vent) is pushing air instead of pulling it out. My Kiln is out in a garage so I don't need a vent so I am not sure how they are set up on an kiln. If is possible for it to be going backwards this could put dust into the air. Hope this isn't pure stupid. But it might be. oh well. Hope you find the solution. and Happy firing. Link to comment Share on other sites More sharing options...
Lucille Oka Posted November 7, 2012 Report Share Posted November 7, 2012 I agree with the other possibilities, and also be very careful not to allow your vessels to lay against the kiln walls during the bisque fire. And be careful not to bump the brick walls while loading. Link to comment Share on other sites More sharing options...
CPT Posted November 7, 2012 Author Report Share Posted November 7, 2012 thanks for the tips, everyone~ I will have to try putting a shelf on top of my work, good idea! Hopefully it's just the lid. Will have to take a look at it. Don't have a vent system.....just lots of fans and open windows in my studio. Link to comment Share on other sites More sharing options...
perkolator Posted November 7, 2012 Report Share Posted November 7, 2012 i would take a guess that there might have been some loose soft brick dust sitting on the top edge of the kiln walls (from lid rubbing it, or from user touching the brick when loading/unloading), then when you closed the lid the slight woosh of air blew some of the dust inward on the piece. do you have pics of the firebrick contaminants? usually you can tell where the firebrick came from just from what it looks like - since many lids have a refractory mortar coating on them, the brick looks different than those found on the walls. also, you said your kiln doesn't have a vent, but does it have vent intake holes in the lid? Link to comment Share on other sites More sharing options...