Does anyone know what proportions of potash feldspar and nephelline syenite can be used to replace FFF feldspar in a glaze recipe. FFF feldspar does not seem to be available in Australia?

Share this post


Link to post
Share on other sites
Guest JBaymore

Can you post the typical analysis of the FFF feldspar you mention? If you do, I can recalculate it using other materials.

 

But to really be accurate I would also need the typical analysis of your OTHER raw materials that might be used to substitute..... the Neph. SY. and so on.

 

best,

 

.......................john

Share this post


Link to post
Share on other sites

Can you post the typical analysis of the FFF feldspar you mention? If you do, I can recalculate it using other materials.

 

But to really be accurate I would also need the typical analysis of your OTHER raw materials that might be used to substitute..... the Neph. SY. and so on.

 

best,

 

.......................john

 

Thanks so much for the offer of help, I am a new hobby potter and using the lovely new book from Linda Bloomfield called : Colour in glazes, I do not have the precise composition of my materials from my supplier but, Am happy to test, test test.

 

 

The FFF FELDSPAR IS: SiO2 67.7, Al2O3 18.9, , Fe2O3 0.16, CaO 0.72, K2O 7.62, Na2o 4.84 LOI 0.05.

 

The Potash Feldspar is: SiO2 65.8, Al2O3 18.5, Fe2O3 0.1, CaO 0.38, K2O 12, Na2o 2.89, LOI 0.33

 

The Nephaline Syenite is: SiO2 60.5, Al2O3 23 , Fe2O3 0.1, CaO 1, K2O 1, Na2o 10.2 , LOI 0.2

 

I also have a problem with the rutile pink glaze from the book, , come , 8 oxidised, but is firing clear. the recipe is:

 

Any hints gratefully received.

 

Nephelline Syenite. 26

Whiting. 12

Lithium carb. 10

Barium carb. 3

Calcium borate fruit. 5

Quartz. , 44

 

+

 

Rutile. 1.5

Tin oxide. 4

 

Kind regards

 

Jan

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.