lcar Posted October 1, 2012 Report Share Posted October 1, 2012 Hi everyone, It's starting to rain here in northern BC, and this marks the start of me "hunkering down for the winter" as it won't be long before the snow flies. I'm looking especially forward to this winter as I have just bought a small test kiln and my goal is obsess on glaze testing and furthering my glaze chemistry education. I've spent a good part of the last month digging three types of clay of various firing temperatures, as well as have gathered some rather interesting potential glaze materials. Yesterday was day one and I so happy to find my glaze program is now online. After losing my laptops in a break in last spring. It's back to square one, putting my glaze recipes into the computer. I am now also keeping copies of them in google drive. my question is for those who are often working with and comparing recipes. What is your favorite way to list the materials? (aside from the additions). Many recipes seem to put the larger amounts first. Some seem to put the fluxes and then the glass formers. Alphabetical would also make sense to make it easy to compare, I thought. I have the chance here to have all my recipes entered the same and would love to hear how others prefer it, or is there a standard in the ceramics programs? Leanna Link to comment Share on other sites More sharing options...
neilestrick Posted October 1, 2012 Report Share Posted October 1, 2012 I usually list feldspars first, as they are often the largest component, then other fluxes, then clay, then silica last. Just the way I do it, because the feldspars and other fluxes will have the greatest effect on the look of the glaze, so I like to see them first so I can quickly get an idea of what type of glaze I'm dealing with. But many people just go in order of quantity, from largest to smallest. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted October 4, 2012 Report Share Posted October 4, 2012 I agree with Neil. I think that progression comes from the old way of doing glaze calculation math with the Radicals in that order. usually you calculate the fluxes first as they determine the character of the glaze. Marcia Link to comment Share on other sites More sharing options...
lcar Posted October 9, 2012 Author Report Share Posted October 9, 2012 Thanks Neil, Thanks Marcia. I am proceeding as advised and appreciate this forum. Leanna Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.