format of glaze recipes

Recommended Posts

lcar    1

Hi everyone,

 

It's starting to rain here in northern BC, and this marks the start of me "hunkering down for the winter" as it won't be long before the snow flies. I'm looking especially forward to this winter as I have just bought a small test kiln and my goal is obsess on glaze testing and furthering my glaze chemistry education. I've spent a good part of the last month digging three types of clay of various firing temperatures, as well as have gathered some rather interesting potential glaze materials.

 

Yesterday was day one and I so happy to find my glaze program is now online. After losing my laptops in a break in last spring. It's back to square one, putting my glaze recipes into the computer. I am now also keeping copies of them in google drive.

 

my question is for those who are often working with and comparing recipes. What is your favorite way to list the materials? (aside from the additions). Many recipes seem to put the larger amounts first. Some seem to put the fluxes and then the glass formers. Alphabetical would also make sense to make it easy to compare, I thought. I have the chance here to have all my recipes entered the same and would love to hear how others prefer it, or is there a standard in the ceramics programs?

 

Leanna

Share this post


Link to post
Share on other sites
neilestrick    1,380

I usually list feldspars first, as they are often the largest component, then other fluxes, then clay, then silica last. Just the way I do it, because the feldspars and other fluxes will have the greatest effect on the look of the glaze, so I like to see them first so I can quickly get an idea of what type of glaze I'm dealing with. But many people just go in order of quantity, from largest to smallest.

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

I agree with Neil. I think that progression comes from the old way of doing glaze calculation math with the Radicals in that order.

usually you calculate the fluxes first as they determine the character of the glaze.

 

Marcia

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×