Iforgot Posted August 25, 2012 Report Share Posted August 25, 2012 Hey pot people, I was wondering the amount of sodium sillicate and such to make a terra sig with one pound of xx saggar ball clay? Thank you! Darrel Link to comment Share on other sites More sharing options...
Marcia Selsor Posted August 25, 2012 Report Share Posted August 25, 2012 Hey pot people, I was wondering the amount of sodium sillicate and such to make a terra sig with one pound of xx saggar ball clay? Thank you! Darrel I use grams not pounds. Will go check my recipe in the morning but it is just a few drops. What recipe are you using? How are you making the batch? This makes a difference. Let me know what preparation technique you plan to use. I use a few drops of Darvon 7 Marcia Link to comment Share on other sites More sharing options...