The Chinese used to use a high calcium product that make painting in the tortoise shell and partridge feather style possible. I would suggest exploring that.

- h a n s e n

Share this post


Link to post
Share on other sites

I need to create a set of dishes using temoku with another glaze. Any suggestions?

 

 

I like accents with John Reeves Chrome Green.

 

REEVES GREEN cone 10 reduction

CUSTER 75.0

WHITING 15.0

FLINT 5.0

KAOLIN 5.0

CHROME OXIDE 4.0

 

Or, if you'd like something tradtional, put Nuka at the top.

 

*Phil Roger's Synthetic Nuka

 

Potspar 35.6

Whiting 21.8

Talc 2

Bone Ash 2

Ball Clay 5.9

Flint 29.7

ferro3134 3 (I have subbed wood ash) *

 

See photo here: Nuka over Tenmoku

http://images21.fotki.com/v760/photos/1/199764/814063/AUT_0020-vi.jpg

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.