Jump to content


Photo

slipresist recipe


  • Please log in to reply
4 replies to this topic

#1 naghmeh

naghmeh

    Member

  • Members
  • PipPip
  • 26 posts

Posted 24 April 2012 - 03:43 AM

i want recipes for slip resist to make it

anybody help me??

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,349 posts
  • LocationRed Lodge, Montana

Posted 24 April 2012 - 05:58 AM

Could you explain what you are trying to do? I am not sure I understand what you mean by slip resist.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 naghmeh

naghmeh

    Member

  • Members
  • PipPip
  • 26 posts

Posted 29 April 2012 - 05:43 AM

Could you explain what you are trying to do? I am not sure I understand what you mean by slip resist.

Marcia



i want to use for raku, but i don't have slip resist. how can i get or make it???

#4 atanzey

atanzey

    -

  • Members
  • PipPipPip
  • 147 posts
  • LocationSouth-Central Pennsylvania

Posted 29 April 2012 - 07:20 AM

I think we're confused by your terminology. To me, 'slip' and 'resist' don't go together. However, I assume you're looking for the 'resist' part. I use two kinds of wax. Wax resist is a water-bourne wax product that can (mostly) be washed out of brushes (but you have to be quick and through). Paraffin wax is melted, and can be brushed, splattered or dipped.

Wax resist is available commercially from ceramic supply houses, but I don't really think you could make your own. Paraffin is readily available at a grocery store (in the U.S.), or just about any source of clear or white wax would probably work. I'm currently using up a stockpile of white candles that I inherited. It's not as nice as pure paraffin, but it was free.

If you're looking for slip, you can make your own, but I don't use much prepared slip yet, so I can't offer much advice.

#5 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,349 posts
  • LocationRed Lodge, Montana

Posted 29 April 2012 - 12:47 PM

Are you talking about slip used in Naked Clay raku technique?
There are several people you should google or look up in Ceramic Arts Daily.