I would like a specific look for a rabbit on a tile.

I'm looking for a white, or off white, cone 5-6 glaze that will have a Raku look with some lines or crackles. Anyone have any suggestions for a premade commercial glaze to be brushed on?

Thanks.
Gwen

#2 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,304 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 08 April 2012 - 06:11 PM

http://www.ilovetocr...Range Index.pdf
Mark Cortright
www.liscomhillpottery.com

#3 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,114 posts
  • LocationRaleigh, NC

Posted 09 April 2012 - 10:42 AM

Amaco also makes crackle glazes in several colors ... they have an online catalogue.
www.amaco.com


Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#4 Raku

Raku

    Member

  • Members
  • PipPip
  • 16 posts
  • LocationPerth Western Australia

Posted 28 April 2012 - 07:15 PM

I would like a specific look for a rabbit on a tile.

I'm looking for a white, or off white, cone 5-6 glaze that will have a Raku look with some lines or crackles. Anyone have any suggestions for a premade commercial glaze to be brushed on?

Thanks.
Gwen




Frit 3134 2100 grams

Ball Clay 378

Zircon Flour 378



Fire to 1000c - 1080c

When you rech temp spray with find water, then reduce with paper or sawduse for 30min

When cooled re-heat to say 100-150 to open the cracks then use strong tea, coffee or anything dark to empasise the cracks.

I have used this recipe many times.