oldlady Posted May 26, 2018 Report Share Posted May 26, 2018 put the kiln on at 7 pm using my L&L with the setting "slow glaze, cone 6" no hold. used the standard preheat without a hold and checked it just now. the temp is already at 826 0n 1, 792 on 2 and 765 on 3. question, is it going too fast? the work is bisqued and glazed today. Link to comment Share on other sites More sharing options...
oldlady Posted May 26, 2018 Author Report Share Posted May 26, 2018 at 10:20 i reviewed the program and it is slow glaze cone 6 no hold. top 1071 , middle 1061 and bottom 1007. Link to comment Share on other sites More sharing options...