Posted 15 January 2012 - 11:48 PM

I am wanting to do some tri Azial glaze experiments for two reasons One is to further my understanding of glaze ingredients and secondly I want to set them up as a tile display that looks nice and could be used in a class room situation as a study guide of sorts. What books would you recommend or what other sources. Ain't clay fun Kabe

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,207 posts
  • LocationRed Lodge, Montana

Posted 16 January 2012 - 07:11 AM

Here is a website
http://www.matrix200...axialblends.htm
definition
http://ceramicartsda...triaxial-blend/
It does a thorough job of explaining the process.

here is a slide series
http://coloradoartst...ial-glaze-test/
My tri axial info is on old purple ditto hand outs. A similar system from a book might be the grid system from Ian Curry. Look up Ian's books.

marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 Kabe

Kabe

    Advanced Member

  • Members
  • PipPipPip
  • 132 posts
  • LocationMo.

Posted 16 January 2012 - 09:32 AM

Thank you Marcia. Hope your Raku is going well. ain't clay fun Kabe