I'm looking for an ultra low-fire clear glaze as I want to dip my toe in kutani yuri-kinsai.. I found an interesting cone 014 recipe that is about 25% frit p-54, and I cant find any for sale online.  Can anyone suggest either a suitable replacement for frit p-54 or an alternate low/fast-fire clear glaze that is suitable for yuri-kinsai?

This is the glaze I was going to roll the dice with:

 

Frit 3269 44    
Frit P-54 26    
Silica 14    
Lithium Carbonate 10    
Kaolin (Theoretical) 6

 

 

thanks all!

Share this post


Link to post
Share on other sites

Ferro 3134 is close enough to the Pemco Frit (P-54).

==============================================================
Molecular Formula of Ferro Frit 3134:

	Na2O 	0.317 	B2O3 	0.634	SiO2 	1.476	CaO 	0.683

Percentage Analysis (weight %)

	46.50 %	 	SiO2
	10.30 % 	Na2O
	20.10 % 	CaO
	23.10 % 	B2O3
	_____________________
	100 % 		TOTAL
=================================================================
Molecular Formula of Pemco Frit P-54:

	Na2O  0.320	B2O3   0.635	SiO2  1.457	CaO   0.680

Percentage Analysis (weight %)

	 46.17 % 	SiO2 
	 10.46 % 	Na2O 
	 20.12 % 	CaO  
	 23.26 % 	B2O3 
	_____________________
	100 % 		TOTAL

=================================================================

Edited by Sputty
Eventually got my act together. Blame Audrey Hepburn.
mousey likes this

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.