Hi,

I was wondering if any one out there has used rubber cement as a glaze resist and if so, how well did it work?


Thanks

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,117 posts
  • LocationRaleigh, NC

Posted 18 May 2010 - 10:22 AM

Interesting idea ... I would think offhand that it would pull off too easily once you got it damp.

Have you tried it since you posted this question? If it works it could be cheaper than using liquid latex.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#3 AndyL

AndyL

    Advanced Member

  • Members
  • PipPipPip
  • 167 posts
  • LocationNJ, USA

Posted 18 May 2010 - 07:48 PM

I use latex resists not rubber cement but it's certainly an interesting idea. Why not try making a few pinch pots and experiment a little with this??

#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,359 posts
  • LocationRed Lodge, Montana

Posted 18 July 2010 - 01:24 PM

I use rubber latex from Amaco. If it gets dry it is tough to pull off. I found if I dampen it, it comes off much easier. I dilute it for a painterly application onto bisque.