Guest Posted June 27, 2017 Report Share Posted June 27, 2017 What is a good ratio of Alumina Hydrate to wax resist? 1:2? TIA Link to comment Share on other sites More sharing options...
Dick White Posted June 27, 2017 Report Share Posted June 27, 2017 My ratio is some alumina in some wax. No specific measurement, but add enough that you can detect it in the wax coating. The alumina will settle so keep it stirred. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 27, 2017 Report Share Posted June 27, 2017 I usually put a few teaspoons in a small commercial bottle like a pint. 5-10% should do it. Marcia Link to comment Share on other sites More sharing options...