Kaolinwasher Posted February 3, 2017 Report Share Posted February 3, 2017 I have been making porcelain, and i was using regular bentonite, and noticed dark specks in the clay after firing , wo i decided to mix three grams up in to one cup of water and stir it for three days off and on but what i found out was after i poorer it into my clay test all the heavy junk settled and never made it into my clay body- so now i know this stuff is not so refined not that it can't do the job, I am just going to have to wash it real thin and let the junk settle you can see the black grit in the bottom of the cup Link to comment Share on other sites More sharing options...
neilestrick Posted February 3, 2017 Report Share Posted February 3, 2017 Regular bentonite is not good for porcelain. There are whiter options out there. Link to comment Share on other sites More sharing options...