I inherited a small amount of Albany slip and Barnard Blackbird slip in powder form - about 2 cups of each. I am working with stoneware and firing at cone 6 in an electric kiln. As I am new at this, are there easy recipes for these two slips anyone cares to share? These slips are best applied to wet, leatherhard or bisque ware?

Link to comment
Share on other sites

post-1954-0-29530200-1473849349_thumb.jpgHere are 2 recipes. I use the first one. The mug on the right has this glaze on the inside and top.

 

 

Andie’s Handful of Earth **(I use this with my cobalt green)

Red Art          50

Bernard Slip             25

#3134                             50

 

Glossy brick red breaking black and dark brown

great on porcelain , nice on stoneware

 

Old Gold Albany

Lithium Carb           10

Alberta Slip             78

Zircopax        12

NICE, STABLE FAUX SHINO

Red Breaking tan and cream

 

Marcia

 

 

post-1954-0-29530200-1473849349_thumb.jpg

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.