Bill T. Posted August 11, 2011 Report Share Posted August 11, 2011 I am using Tony Hansen's base glaze and adding stains for some of my colors. I like to brush much of my glaze and this formulation does not flow well to brush. Is there anything I can add to enhance it's brushibility? Or would I be better off to try another base glaze? I also have the same trouble on most of the MC6 glazes. Thanks for the help. Link to comment Share on other sites More sharing options...
bciskepottery Posted August 13, 2011 Report Share Posted August 13, 2011 Here is an article by Pete Pinnell that talks about thinning a glaze for brushing (see part 2). http://www.claytimes.com/articles/glazeadjusting.html Link to comment Share on other sites More sharing options...