Search the Community
Showing results for tags 'Obvara'.
-
From the album: saggar, horse hair, feathers, foil saggars, Obvara
Obvara fire, surface treatment created with sodium silicate on a cylinder then stretched into an orb.-
- obvara
- cracklesurface
-
(and 1 more)
Tagged with:
-
-
-
-
From the album: Raku Firing
-
From Sept. workshop and home firings 2015
Marcia Selsor posted a gallery image in Browse Member Galleries
From the album: New 2015 Obvara
top view of crackled surface fired in Obvara -
From the album: Latest Obvara
-
From the album: Latest Obvara
-
From the album: Latest Obvara
-
From the album: Latest Obvara
-
From the album: saggar, horse hair, feathers, foil saggars, Obvara
crackles, surface and patterns -
From the album: saggar, horse hair, feathers, foil saggars, Obvara
-
From the album: saggar, horse hair, feathers, foil saggars, Obvara
nice dots on the crackles -
From the album: saggar, horse hair, feathers, foil saggars, Obvara
-
From the album: saggar, horse hair, feathers, foil saggars, Obvara
got some interesting results of patterns and surfaces -
From the album: saggar, horse hair, feathers, foil saggars, Obvara
from the obvara firing last week. -
From the album: saggar, horse hair, feathers, foil saggars, Obvara
-
From the album: Up In Smoke Pottery
Obvara vessell, 2013-
- obvara
- alternative pottery
-
(and 1 more)
Tagged with:
-
From the album: Up In Smoke Pottery
Obvara vessel-
- Obvara
- alternative firing
-
(and 1 more)
Tagged with:
-
From the album: saggar, horse hair, feathers, foil saggars, Obvara
Going into brew -
From the album: saggar, horse hair, feathers, foil saggars, Obvara
Hot pot coming out of Flour paste brew. -
From the album: saggar, horse hair, feathers, foil saggars, Obvara
Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water. -
From the album: saggar, horse hair, feathers, foil saggars, Obvara
Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water. Pieces cooling -
From the album: saggar, horse hair, feathers, foil saggars, Obvara
Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water. -
From the album: saggar, horse hair, feathers, foil saggars, Obvara
Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water.