Anyone have a suggestion for storing/displaying glaze sample tiles?
Benzine
In my classroom, I just have a board mounted to the wall, with nails. My tiles have a hole, which allow me to remove the tiles.
Chris Campbell
If you did not put a hole in them simply glue Velcro to the tile and the wall.
High Bridge Pottery
An old cd rack could work. I only have three glazes so mine sit in a small pile.