glazenerd 1,807 Posted April 24, 2017 Report Share Think I figured out a name for this form: Trumpet Vase I see the glazes are laying down nicely on the Soldate 60 now. Quote Link to comment
1515art 260 Posted April 24, 2017 Report Share Soldate loves raku, it's only when you get to cone 6 and above some glaze issues with the new formula and depending on the glaze some at cone 10 can be kind of drab and disappointing depending what I'm hoping for. That's the one thing I love about porcelain they way it fires so vibrant and lively. Quote Link to comment