Mortar and Pestle
Made loosely following a Simon Leach video tutorial
Runyan Wheatstone clay
Waterfall brown dunk, angle dipped in Ron Roy's Clear
Grinding surfaces were left unglazed, and a triangular shelf stilt was used to hold the pestle upright on its unglazed end for glaze firing