This bowl was fired at cone 4 and glazed with Potter's Choice glazes Tourmoline & Iron Lustre to cone 06 in a reduction kiln.


Copyright

© 2013 Deutmeyer Pottery
Sign in to follow this  
From the album:

My pottery

  • 7 images
  • 0 comments
  • 0 image comments

Photo Information for DeutmeyerPottery01


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.