Photo Information for MugsGlazedSpring2018.JPG

Taken with Panasonic DMC-FZ1000

  • 21.4 mm
  • 10/800
  • f f/3.5
  • ISO 160
View all photo EXIF information

Recommended Comments

The handles on these mugs have been extruded with a plastic commercial die in a Putty gun type extruder. I have altered the handle shape to make it thicker, and give a better rib form with more rounded area where the fingers will fit. I also am filling/blending gap at the bottom of the handle where joined to the pot.