Arnold Howard Posted November 2, 2010 Report Share Posted November 2, 2010 Paragon has just finished producing a video on the repair of bulging sidewall elements. The information applies to most brands of kilns. I look forward to your feedback. Sincerely, Arnold Howard Paragon Industries, L.P., Mesquite, Texas USA ahoward@paragonweb.com / www.paragonweb.com Link to comment Share on other sites More sharing options...
BPACH Posted November 2, 2010 Report Share Posted November 2, 2010 Good video. Thanks for educating me. Link to comment Share on other sites More sharing options...
Username Posted November 3, 2010 Report Share Posted November 3, 2010 Hey, this is good timing, as one of my elements just popped out of the wall last week. Now, does Paragon have anything for bulging "tummy elements?" Link to comment Share on other sites More sharing options...