Hello Sabi54.

Nice link. The gal describes the process well. Two differences in my experience:

1) I let the mold purge a full 60 minutes at the end. (50-70 lbs. depending upon the pressure setting of the hydraulic press.)

2) I usually poured in a rigid mold casing made of steel or pvc. (That protected the molds from cracking when the press brought the two molds together.)

Mold duct tubing - the first time I ordered it, without knowing its proper name, I called it "hollow cloth rope". If the rope highlighted, holds its round shape, then I think it might work.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.