divinebread Posted July 15 Report Share Posted July 15 Brand new Paragon Janus 1613 sentinel smartTouch controller by Bartlett Ok I set my initial fire to cone 01 (brand new). No holds. Medium speed. Put witness cone 01 in view of port hole. Per the paragon manual. Check on witness cone 01 to see if it’s all set. Kiln at 1821 degrees per the controller. No longer can see the cone which means it has dropped all the way down. So per the manual I needed to shut it down. So I did. Am I doing this wrong? 😞 Why would it drop the witness come for 01 at 1821 degrees? First personal kiln, first fire at home. Thank you. Quote Link to comment Share on other sites More sharing options...
neilestrick Posted July 15 Report Share Posted July 15 Digital kilns often need calibration. You can do a thermocouple offset or cone offset to dial it in. Quote Link to comment Share on other sites More sharing options...