Sylvie Posted June 14 Report Share Posted June 14 I have a skutt 818. New elements and new thermocouple. There was only 1 test firing done prior. I did a glaze firing using this program and I got a ERR 1 probably at the end of segment 5 or beginning of segment 6. What could be the cause and how to fix it. 1 200 250 F 0 2 400 1000 F 0 3 180 1150 F 0 4 300 1967 F 0 5 120 2200 F 0 6 150 1950 F 30 MIN Quote Link to comment Share on other sites More sharing options...
neilestrick Posted June 14 Report Share Posted June 14 Do a paper test: https://hotkilns.com/support/pottery-kiln-trouble-shooting-actions/paper-troubleshooting-test Check all your thermocouple connections. Quote Link to comment Share on other sites More sharing options...