Katiethepaintinglady Posted April 17 Report Share Posted April 17 I recently had a house fire and many small containers of acrylic paint were subjected to severe heat but not directly burned. Will they be salvageable? Thanks Katiethepaintinglady Quote Link to comment Share on other sites More sharing options...
Rockhopper Posted April 18 Report Share Posted April 18 If there's still any liquid in them, you might be able to use them but, in my experience, re-hydrating dried out acrylics doesn't work. Quote Link to comment Share on other sites More sharing options...