sprestel@verizon.net Posted April 7, 2013 Report Share Posted April 7, 2013 I have a never been used but old kiln sitter type kiln and I wanted to use it in my garage. My garage is attached but there is an air tight door to the house. I didn't want to invest in a vent system yet because the kiln is old and I don't know if or how well it will work. I will leave the garage door open a bit for venting. Is this safe? Thank you, in advance, for your help! Link to comment Share on other sites More sharing options...
Guest JBaymore Posted April 7, 2013 Report Share Posted April 7, 2013 For initial testing..... that should be fine. Make sure that in the garage there are not any cans of oil based paints and thinner and gasoline and such. That could be an issue. Eventually you will want a vent .... it improves the quality of the wares,.....not only takes care if getting the noxious crap out of the space. best, ....................john Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.