cholmes Posted May 16, 2023 Report Share Posted May 16, 2023 Hi there! So my bottom two elements are not working and trying to troubleshoot why. New Relay and all new elements. New thermocouple. Getting power. What else could it be? ANY ideas are welcomed! Thank you! Quote Link to comment Share on other sites More sharing options...
neilestrick Posted May 16, 2023 Report Share Posted May 16, 2023 @cholmes If both elements in one ring are not working then it's usually a bad relay. Are you sure it's wired correctly? Was it working before but now it's not, or is this the first try since replacing the elements and relays? Quote Link to comment Share on other sites More sharing options...
ZAN Ceramics Posted May 17, 2023 Report Share Posted May 17, 2023 Calling Skutt for tech support is fantastic. They will walk you through the whole process. It’s a good reason to buy a Skutt in my opinion. Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.