MarkS Posted December 25, 2011 Report Share Posted December 25, 2011 Curious if anyone has any suggestions about mixing mason stain to add to clay. Before I've mixed it with water and then kneaded into the clay. But I was always seem to get some undissolved stain lumps. Would it work better to add some clay clay to the solution and if so should it be the clay I'm mixing with or EPK, OM-4, etc? Any suggestions as to how to get lumps out? Sieve? Link to comment Share on other sites More sharing options...
bciskepottery Posted December 25, 2011 Report Share Posted December 25, 2011 Blend your Mason stain, water and a small addition of the clay body in a blender (or jar with hand blender) into a smooth slip and then wedge back into your clay. Link to comment Share on other sites More sharing options...