Hi everyone - this is one of the VERY few threads on the internet about Superfire kilns. Seeing that this thread is years old, I do hope someone stumbles upon it again to help a gal out!
I purchased a 240V 50A Superfire kiln (D295) off of Facebook and used it well enough for about a year before the elements needed replacing. I contacted Euclids and they sent me elements for it. The connectors they sent were fairly large - turns out there was some unwanted metal contact. When I turned it on there was some drama and the kiln shut off.
I just got crimp connectors to save some space in the box, and naturally I forgot to label the relays… I have an ohmmeter to measure resistance of the elements but I’m unsure what they’re supposed to be reading since I can’t find any manuals online.
are there any electricians on here that may be able to help me with the math??