Hello all,
I've been getting some mixed results from my electric kiln lately (front loading, Pottery Crafts - 2015).
I'm firing to 1260° C and using witness cones (Orton 7 & 8). Trusting the cones I've been shutting the kiln off at 1220 - 1230° C of late. Feels like a big gap between controller temp and heatwork.
The controller setting is:
1. 120 to 600
2. 250 to 1260
The kiln seems to struggle from 1000, really slows down, and takes a long time to reach target temp. This might be impacting the heatwork? Maybe 250 is too low?
I've been reading up on this and it seems like many set their cut off time of a 1260 firing to 1235 (Clayman Supplies) - 1250 (Stuart Carey), sometimes with a long soak. I find this very confusing.
Any insight would be highly appreciated.
Fyi. The elements are fairly new and we had the kiln looked over by a professional, who found no fault with it.
Hope this makes sense.
Thanks!