For years I’ve used a recipe for “Oribe”, a transparent medium green cone 6 glaze. The last batch I mixed the zinc oxide had formed pellets that wouldn’t go through my sieve. This has happened before with little noticeable effect. This time every piece with Oribe ran and stuck to the kiln wash, and several pieces formed sharp bubbles. Any ideas how to proceed?