no it is in my closet across from my classroom. I can't find anything online about what the lo means but that is the only thing that is on the screen.
-
-
My old, old kilns pyrometer broke so I was told the dual input pyrometer and thermometer would still work in my kiln. I went to try it out and do a test firing but when I click it on it says lo on the screen. I changed the battery when it came in last week because the battery was dead. Any help is greatly appreciated.
Thanks
Brand new dual input pyrometer not working
in Equipment Use and Repair
Posted
@Bill Kielb that was it! Thank you. I haven't had to change one in years so I thought I was doing the installation wrong. Nope it came hooked up wrong. Thanks again!