Virginia Murphy Pottery got a reaction from Hulk in Pinholes: brush-on Western Matte Glaze
Thanks for the reply Hulk! I can’t tell if the holes are making it all the way through unfortunately.
Yes maybe it’s a bit thicker at the foot. could be a thickness problem I suppose.
yea, that’s the amaco iron lustre i mentioned. It was applied the same as the western glaze, and it had no problems. So maybe it’s a glaze thing. Not sure.
that link is suuuuper helpful! Thanks so much!