I'm starting to evaluate the wild clay in my yard in Maple Grove, MN. I've floated off the organic material, and sieved it with a paint strainer bag. It bisqued up nicely, but melted into bubbly baby-poo green at cone 6.
I'm not expecting to make great art with this, just making a statement about how crappy my garden soil is, and get an intuitive understanding of how clay is processed and tested.
My next step is to try it at cone 1 to see if I can use it as earthenware, and maybe try it as a slip over a high-fire clay body.
I have 2 pieces that I'm going to raku fire on Thursday, weather permitting. If it can take bisque it can take raku.
Wild Clay Processing
in Clay and Glaze Chemistry
Posted
I'm starting to evaluate the wild clay in my yard in Maple Grove, MN. I've floated off the organic material, and sieved it with a paint strainer bag. It bisqued up nicely, but melted into bubbly baby-poo green at cone 6.
I'm not expecting to make great art with this, just making a statement about how crappy my garden soil is, and get an intuitive understanding of how clay is processed and tested.
My next step is to try it at cone 1 to see if I can use it as earthenware, and maybe try it as a slip over a high-fire clay body.
I have 2 pieces that I'm going to raku fire on Thursday, weather permitting. If it can take bisque it can take raku.