I have had many negative results with Standard 112. It is too soft to throw and incredibly short . I’ve been trying to teach classes with it and have seen my students struggle. I just unloaded the best load and many of my handbuilt mugs have warped . I’ve been doing Pottery for 25 years and I’ve never had this situation. Super disappointed.